China · GB

20

GB/T 8162:1999 — Seamless steel tubes for structural purposes

Chemical composition

wt% · log scale
0.010.11C0.17 – 0.23Cr0.25Cu0.25Mn0.35 – 0.65Ni0.3P0.035S0.035Si0.17 – 0.37
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≤225 MPaTensile strength Rm≤390 MPaElongation A≤20 %

Chemical composition

ElementminmaxSimilarRemarks
C0.170.23
Cr0.25
Cu0.25
Mn0.350.65
Ni0.3
P0.035
S0.035
Si0.170.37

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
seamless steel tube, hot rolled, heat treated≤225≤390≤20