China · GB

20

GB/T 32958:2016 — Stainless steel clad pipes for fluid transport

Chemical composition

wt% · log scale
0.010.11C0.17 – 0.23Cr0.25Cu0.25Mn0.35 – 0.65Ni0.3P0.035S0.035Si0.17 – 0.37
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥235 MPaTensile strength Rm≥390 MPasteel tubesElongation A≥19 %steel tubes, d <= 168.3mmElongation A≥19 %steel tubes, d > 168.3mm

Chemical composition

ElementminmaxSimilarRemarks
C0.170.23
Cr0.25
Cu0.25Copper in steel for hot working shall not exceed 0.20%
Mn0.350.65
Ni0.3
P0.035
S0.035
Si0.170.37

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel tubes≥235≥390
steel tubes, d <= 168.3mm≥19
steel tubes, d > 168.3mm≥19