China · GB

20

GB/T 3639:2000 — Seamless cold-drawn or cold-rolled steel tubes for precision applications

Chemical composition

wt% · log scale
0.010.11C0.17 – 0.23Cr0.25Cu0.25Mn0.35 – 0.65Ni0.3P0.035S0.035Si0.17 – 0.37
  • min – max range
  • typical value

Mechanical properties

value range by condition
Tensile strength Rm≥510 MPaElongation A≥5 %Tensile strength Rm≥510 MPaElongation A≥5 %cold drawn seamless tubeTensile strength Rm≥510 MPaElongation A≥5 %cold drawn seamless tube, annealed

Chemical composition

ElementminmaxSimilarRemarks
C0.170.23
Cr0.25
Cu0.25
Mn0.350.65
Ni0.3
P0.035
S0.035
Si0.170.37

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
cold drawn seamless tube≥510 Non-standard data, for reference only≥5 Non-standard data, for reference only
cold drawn seamless tube, annealed≥510 Non-standard data, for reference only≥5 Non-standard data, for reference only