China · GB

20

GB/T 3094:2012 — Cold drawn shaped steel tubes

Chemical composition

wt% · log scale
0.010.11C0.17 – 0.23Cr0.25Cu0.25Mn0.35 – 0.65Ni0.3Si0.17 – 0.37
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥245 MPaTensile strength Rm≥410 MPaElongation A≥20 %

Chemical composition

ElementminmaxSimilarRemarks
C0.170.23
Cr0.25
Cu0.25
Mn0.350.65
Ni0.3
Si0.170.37

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel tubes, cold drawn≥245≥410≥20