GB 9948:2006 — Seamless steel tubes for petroleum cracking

Chemical composition

wt% · log scale
0.010.11C0.17 – 0.23Cr0.25Cu0.2Mn0.35 – 0.65Mo0.15Ni0.25P0.03S0.02Si0.17 – 0.37V0.08
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥195 MPasteel tubes 16 < t ≤ 30mm, normalizedYield strength Rp0.2≥185 MPasteel tubes t > 30mm, normalizedYield strength Rp0.2≥205 MPasteel tubes t ≤ 16mm, normalizedTensile strength Rm410–550 MPaImpact energy Kv/Ku≤35 JElongation A≤24 %steel tubes, normalized

Chemical composition

ElementminmaxSimilarRemarks
C0.170.23
Cr0.25
Cu0.2
Mn0.350.65
Mo0.15
Ni0.25
P0.03
S0.02
Si0.170.37
V0.08

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel tubes 16 < t ≤ 30mm, normalized≥195
steel tubes t > 30mm, normalized≥185
steel tubes t ≤ 16mm, normalized≥205
steel tubes, normalized410–550≤24≤35

Heat treatment

Type3
Heat-treatment processNormalized