China · GB
20
GB/T 710:1991 — Hot-rolled quality carbon structural steel sheets and strips
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.17 | 0.23 | ||
| Cr | 0.25 | |||
| Cu | 0.25 | |||
| Mn | 0.35 | 0.65 | ||
| Ni | 0.3 | |||
| P | 0.035 | |||
| S | 0.035 | |||
| Si | 0.17 | 0.37 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| hot rolled steel plates, steel strip, heat treated | 355–500 Non-standard data, for reference only;355–490 Non-standard data, for reference only | ≥24 Ordinary deep-drawn grade.A is δ10 value; non-standard data, for reference only;≥24 Deep deep-drawn grade.A is δ10 value; non-standard data, for reference only;≥25 Most deep deep-drawn grade.A is δ10 value; non-standard data, for reference only |