Italy · UNI

C 55

UNI 8893:1986 — UNI 8893

Chemical composition

wt% · log scale
0.010.1110C0.52 – 0.6Mn0.6 – 0.9P0.035S0.035Si0.15 – 0.4
  • min – max range
  • typical value

Chemical composition

ElementminmaxSimilarRemarks
C0.520.6
Mn0.60.9
P0.035
S0.035
Si0.150.4

Fatigue

Test conditions
ItemDetail
ProductSemi Finished products; Thickness: <= 16 mm; +QT
ExperimentReversed bending; T: 20°C
Specimen
Monotonic
PropertyValue
Yield strength (MPa)550.0
Tensile strength (MPa)800.0 950.0
Elongation (%)12.0
Reduction of area (%)30.0
Stress life
No.Cycles
11E7

Heat treatment

Type1
Heat-treatment curveHardness-Tempering