United Kingdom · B.S.
1.4563
BS EN 10250-4 — Open steel die forgings for general engineering purposes.Part 4:Stainless steels
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionHigh / low temperature
value vs. temperature- forgings Solution annealed · Yield strength Rp0.2
Physical properties
vs. temperatureChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.02 | |||
| Cr | 26 | 28 | ||
| Cu | 0.7 | 1.5 | ||
| Mn | 2 | |||
| Mo | 3 | 4 | ||
| N | 0.11 | |||
| Ni | 30 | 32 | ||
| P | 0.03 | |||
| S | 0.01 | |||
| Si | 0.7 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| die forgings, forgings, Solution annealed, <= 250 mm, forged bars | 220 | 500 750.00 | 30 | 60;100 |
Physical properties
20.0
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 195.00 | 12.00 | 450.00 | 1.00 | 8.00 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 7.61–8.10 | 190.00–215.00 | 0.27–0.30 | Typical material properties for stainless steel. These values are not taken from the standard; they are indicative and must not be used for design. |
| 7.86 | 190.00–210.00 | 0.27–0.30 | Material properties for low-carbon, high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design. |
High/low temperature
| Condition | Temperature ℃ | min |
|---|---|---|
| forgings Solution annealed | 550 | 115 |
| forgings Solution annealed | 500 | 120 |
| forgings Solution annealed | 450 | 125 |
| forgings Solution annealed | 400 | 135 |
| forgings Solution annealed | 350 | 145 |
| forgings Solution annealed | 300 | 150 |
| forgings Solution annealed | 250 | 155 |
| forgings Solution annealed | 200 | 160 |
| forgings Solution annealed | 150 | 175 |
| forgings Solution annealed | 100 | 190 |
Similar grades
| Grade | Region | System |
|---|---|---|
| 1.4563 | UNI | |
| X 1 NiCrMoCu 31 27 4 | UNI | |
| 1.4563 | UNE | |
| X 1 NiCrMoCu 31 27 4 | UNE | |
| 1.4563 | STAS | |
| X 1 NiCrMoCu 31 27 4 | STAS | |
| 1.4563 | SS | |
| X 1 NiCrMoCu 31 27 4 | SS | |
| 1.4563 | SNV | |
| X 1 NiCrMoCu 31 27 4 | SNV | |
| 1.4563 | SFS | |
| X 1 NiCrMoCu 31 27 4 | SFS | |
| 1.4563 | PN | |
| X 1 NiCrMoCu 31 27 4 | PN | |
| 1.4563 | ONORM | |
| X 1 NiCrMoCu 31 27 4 | ONORM | |
| 1.4563 | NS | |
| X 1 NiCrMoCu 31 27 4 | NS | |
| 1.4563 | NBN | |
| X 1 NiCrMoCu 31 27 4 | NBN | |
| 1.4563 | MSZ | |
| X 1 NiCrMoCu 31 27 4 | MSZ | |
| 1.4563 | Czech Republic | CSN |
| X 1 NiCrMoCu 31 27 4 | Czech Republic | CSN |
| 1.4563 | Bulgaria | BDS |
| X 1 NiCrMoCu 31 27 4 | Bulgaria | BDS |
| X 1 NiCrMoCu 31 27 4 | B.S. | |
| 1.4563 | AFNOR NF | |
| X 1 NiCrMoCu 31 27 4 | AFNOR NF | |
| X 1 NiCrMoCu 31 27 4 | DIN | |
| 1.4563 | DIN |