Italy · UNI

X 2 CrNiMoN 17 13 3

UNI EN 10088-1 — Stainless steels—Part 1:List of stainless steels

Chemical composition

wt% · log scale
0.0010.010.1110100C0.03Cr16.5 – 18.5Mn2Mo2.5 – 3N0.12 – 0.22Ni11 – 14P0.045S0.015Si1
  • min – max range
  • typical value

Physical properties

vs. temperature
Elastic modulus GPa
165 – 200°C
Mean thermal expansion 10⁻⁶/K
16.0 – 18.0°C

Chemical composition

ElementminmaxSimilarRemarks
C0.03
Cr16.518.5
Mn2
Mo2.53
N0.120.22
Ni1114For special reasons (minimize the delta ferrite content) the maximum content of Ni= 1
P0.045
S0.015
Si1

Physical properties

20.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
200.0015.00500.000.758.00

Typical physical values

DensityElastic modulusPoisson's ratioRemarks
7.61–8.10190.00–215.000.27–0.30Typical material properties for stainless steel. These values are not taken from the standard; they are indicative and must not be used for design.
7.86190.00–210.000.27–0.30Material properties for low-carbon, high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design.

Similar grades

GradeRegionSystem
X2CrNiMoN17-13-3International standardISO
1.4429ItalyUNI
1.4429SpainUNE
1.4429RomaniaSTAS
X 2 CrNiMoN 17 13 3RomaniaSTAS
1.4429SwedenSS
X 2 CrNiMoN 17 13 3SwedenSS
1.4429SwitzerlandSNV
X 2 CrNiMoN 17 13 3SwitzerlandSNV
1.4429FinlandSFS
X 2 CrNiMoN 17 13 3FinlandSFS
1.4429PolandPN
X 2 CrNiMoN 17 13 3PolandPN
1.4429AustriaONORM
X 2 CrNiMoN 17 13 3AustriaONORM
1.4429NorwayNS
X 2 CrNiMoN 17 13 3NorwayNS
1.4429BelgiumNBN
X 2 CrNiMoN 17 13 3BelgiumNBN
1.4429HungaryMSZ
X 2 CrNiMoN 17 13 3HungaryMSZ
1.4429Czech RepublicCSN
X 2 CrNiMoN 17 13 3Czech RepublicCSN
1.4429BulgariaBDS
X 2 CrNiMoN 17 13 3BulgariaBDS
1.4429United KingdomB.S.
X 2 CrNiMoN 17 13 3United KingdomB.S.
1.4429FranceAFNOR NF
X 2 CrNiMoN 17 13 3SpainUNE
X 2 CrNiMoN 17 13 3FranceAFNOR NF
X 2 CrNiMoN 17 13 3GermanyDIN
1.4429GermanyDIN