Sweden · SS

CW506L

SS EN 12163

Chemical composition

wt% · log scale
0.010.11101001000Al0.02Cu66 – 68Fe0.05Ni0.3Pb0.05Sn0.1Total Others0.1
  • min – max range
  • typical value

Mechanical properties

value range by condition
HardnessHVHardnessHBsteel bars, H085, > 4 < 80 mmHardnessHVHardnessHBsteel bars, H115, > 4 < 40 mmHardnessHVHardnessHBsteel bars, H145, > 4 < 10 mmYield strength Rp0.2120 MPaTensile strength Rm≥310 MPaElongation A≥27 %steel bars, R310, > 4 < 80 mm

Chemical composition

ElementminmaxSimilarRemarks
Al0.02
Cu6668
Fe0.05
Ni0.3
Pb0.05
Sn0.1
Total Others0.1
Zn​​Bal​​

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel bars, H085, > 4 < 80 mmHV 90–120;HB 85–115
steel bars, H115, > 4 < 40 mmHV 120–150;HB 115–145
steel bars, H145, > 4 < 10 mmHV ≥150;HB ≥145
steel bars, R310, > 4 < 80 mm120≥310≥27
steel bars, R370, > 4 < 40 mm320≥370≥10
steel bars, R460, > 4 < 10 mm420≥460

Physical properties

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
8.50

Similar grades

GradeRegionSystem
CW506LItalyUNI
CW506LSpainUNE
CuZn33SpainUNE
CW506LSwitzerlandSNV
CuZn33SwitzerlandSNV
CW506LFinlandSFS
CuZn33FinlandSFS
CW506LPolandPN
CuZn33PolandPN
CW506LAustriaONORM
CuZn33AustriaONORM
CW506LNorwayNS
CuZn33NorwayNS
CW506LBelgiumNBN
CuZn33BelgiumNBN
CW506LHungaryMSZ
CuZn33HungaryMSZ
CW506LGermanyDIN
CW506LCzech RepublicCSN
CuZn33Czech RepublicCSN
CW506LUnited KingdomB.S.
CW506LBulgariaBDS
CuZn33BulgariaBDS
CW506LRomaniaASRO
CuZn33RomaniaASRO
CW506LFranceAFNOR NF
CuZn33FranceAFNOR NF
CuZn33ItalyUNI
CuZn33United KingdomB.S.
CuZn33SwedenSS
CuZn 33GermanyDIN