China · GB

15

GB/T 699:2015 — Quality carbon structure steels

Chemical composition

wt% · log scale
0.010.11C0.12 – 0.18Cr0.25Cu0.25Mn0.35 – 0.65Ni0.3P0.035S0.035Si0.17 – 0.37
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥225 MPaTensile strength Rm≥375 MPaElongation A≥27 %Reduction of area Z≥55 %steel bars, normalized, d = 25 mm, d - specimenHardnessHBsteel bars, hot rolled or , d = 25 mm, d - specimen

Chemical composition

ElementminmaxSimilarRemarks
C0.120.18
Cr0.25
Cu0.25Copper in steel for hot working shall not exceed 0.20%
Mn0.350.65
Ni0.3
P0.035
S0.035
Si0.170.37

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel bars, normalized, d = 25 mm, d - specimen≥225≥375≥27≥55
steel bars, hot rolled or , d = 25 mm, d - specimenHB ≤143

Heat treatment

Type34
Heat-treatment processNormalized920℃±30℃, Holding not less than 30min, air-cooled