Czech Republic · CSN
CuNi30Mn1Fe
CSN EN 12452
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionCreep properties
- 1000.0h
Temperature °C · time at rupture
Chemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.05 | |||
| Co | 0.1 | The Cobalt content Co=max 0.1% is included as Ni content. | ||
| Cu | Bal | |||
| Fe | 0.4 | 1 | ||
| Mn | 0.5 | 1.5 | ||
| Ni | 30 | 32 | ||
| P | 0.02 | |||
| Pb | 0.02 | |||
| S | 0.05 | If the purchaser requires the product to be welded | ||
| Sn | 0.05 | |||
| Total Others | 0.2 | |||
| Zn | 0.5 | If the purchaser requires the product to be welded |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| Seamless tubes, H085 | HV ≥85 | |||||
| Seamless tubes, R370 | ≥120 | ≥370 | ≥35 |
Physical properties
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 8.90 |
Creep
| Temperature ℃ | Time h | Rp0.1 |
|---|---|---|
| 350 | 1000.0h | 139.0 |
| 450 | 1000.0h | 55.8 |
| 550 | 1000.0h | 4.6 |
Similar grades
| Grade | Region | System |
|---|---|---|
| CW354H | UNI | |
| CW354H | UNE | |
| CuNi30Mn1Fe | UNE | |
| CW354H | SS | |
| CW354H | SNV | |
| CuNi30Mn1Fe | SNV | |
| CW354H | SFS | |
| CuNi30Mn1Fe | SFS | |
| CW354H | PN | |
| CuNi30Mn1Fe | PN | |
| CW354H | ONORM | |
| CuNi30Mn1Fe | ONORM | |
| CW354H | NS | |
| CuNi30Mn1Fe | NS | |
| CW354H | NBN | |
| CuNi30Mn1Fe | NBN | |
| CW354H | MSZ | |
| CuNi30Mn1Fe | MSZ | |
| CW354H | DIN | |
| CW354H | Czech Republic | CSN |
| CW354H | B.S. | |
| CW354H | Bulgaria | BDS |
| CuNi30Mn1Fe | Bulgaria | BDS |
| CW354H | ASRO | |
| CuNi30Mn1Fe | ASRO | |
| CW354H | AFNOR NF | |
| CuNi30Mn1Fe | UNI | |
| Cu-Ni30Mn1Fe | AFNOR NF | |
| CuNi30Mn1Fe | B.S. | |
| CuNi30Mn1Fe | SS | |
| CuNi30Mn1Fe | DIN |