Belgium · NBN

CW714R

NBN EN 12164

Chemical composition

wt% · log scale
0.010.1110100Cu59 – 61Fe0.1Ni0.3Pb0.4 – 1Sn0.5 – 1Total Others0.2
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2200 MPaTensile strength Rm≥360 MPaElongation A≥25 %HardnessHB+R360 50 < d < 80mmYield strength Rp0.2220 MPaTensile strength Rm≥370 MPaElongation A≥22 %HardnessHB+R370 25 < d < 50mmYield strength Rp0.2240 MPaTensile strength Rm≥390 MPaElongation A≥18 %HardnessHB+R390 12 < d < 25mmYield strength Rp0.2250 MPaTensile strength Rm≥410 MPaElongation A≥18 %HardnessHB+R410 2 < d < 50mm

Chemical composition

ElementminmaxSimilarRemarks
Cu5961
Fe0.1
Ni0.3
Pb0.41
Sn0.51
Total Others0.2
Zn​​Bal​​

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
+R360 50 < d < 80mm200≥360≥25HB ≤110
+R370 25 < d < 50mm220≥370≥22HB ≤110
+R390 12 < d < 25mm240≥390≥18HB ≤120
+R410 2 < d < 50mm250≥410≥18HB ≤125
+R460 2 < d < 25mm350≥460≥10HB ≤140
+R500 2 < d < 12mm400≥500≥5HB ≤160

Physical properties

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
8.40

Similar grades

GradeRegionSystem
CW714RItalyUNI
CW714RSpainUNE
CuZn37Pb1Sn1SpainUNE
CW714RSwedenSS
CW714RSwitzerlandSNV
CuZn37Pb1Sn1SwitzerlandSNV
CW714RFinlandSFS
CuZn37Pb1Sn1FinlandSFS
CW714RPolandPN
CuZn37Pb1Sn1PolandPN
CW714RAustriaONORM
CuZn37Pb1Sn1AustriaONORM
CW714RNorwayNS
CuZn37Pb1Sn1NorwayNS
CuZn37Pb1Sn1BelgiumNBN
CW714RHungaryMSZ
CuZn37Pb1Sn1HungaryMSZ
CW714RGermanyDIN
CW714RCzech RepublicCSN
CuZn37Pb1Sn1Czech RepublicCSN
CW714RUnited KingdomB.S.
CW714RBulgariaBDS
CuZn37Pb1Sn1BulgariaBDS
CW714RRomaniaASRO
CuZn37Pb1Sn1RomaniaASRO
CW714RFranceAFNOR NF
CuZn37Pb1Sn1FranceAFNOR NF
CuZn37Pb1Sn1ItalyUNI
CuZn37Pb1Sn1United KingdomB.S.
CuZn37Pb1Sn1SwedenSS
CuZn37Pb1Sn1GermanyDIN