Chemical composition

wt% · log scale
0.010.1110Cr0.05 – 0.25Cu0.1Fe0.4Mg4 – 4.9Mn0.4 – 1Si0.4Ti0.15Total Each0.05Total Others0.15Zn0.25
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥110 MPaTensile strength Rm≥270 MPaElongation A≥12 %Extruded bars/rods, Annealed +O, <= 200 mm +D; <= 200 mm +T +T - thickness; +A - areaYield strength Rp0.2≥125 MPaTensile strength Rm≥270 MPaElongation A≥12 %Extruded bars/rods, Strain-hardened only +H111, <= 200 mm +D; <= 200 mm +T +T - thickness; +A - areaYield strength Rp0.2≥110 MPaTensile strength Rm≥270 MPaElongation A≥12 %Extruded bars/rods +H112, <= 200 mm +D; <= 200 mm +T +T - thickness; +A - areaYield strength Rp0.2≥110 MPaTensile strength Rm≥270 MPaElongation A≥12 %Extruded bars/rods +F, <= 200 mm +D; <= 200 mm +T +T - thickness; +A - area

Physical properties

vs. temperature
Mean thermal expansion 10⁻⁶/K
22.3 – 26.0°C

Chemical composition

ElementminmaxSimilarRemarks
Al​​Bal​​
Cr0.050.25
Cu0.1
Fe0.4
Mg44.9
Mn0.41
Si0.4
Ti0.15
Total Each0.05
Total Others0.15
Zn0.25

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Extruded bars/rods, Annealed +O, <= 200 mm +D; <= 200 mm +T +T - thickness; +A - area≥110≥270≥12
Extruded bars/rods, Strain-hardened only +H111, <= 200 mm +D; <= 200 mm +T +T - thickness; +A - area≥125≥270≥12
Extruded bars/rods +H112, <= 200 mm +D; <= 200 mm +T +T - thickness; +A - area≥110≥270≥12
Extruded bars/rods +F, <= 200 mm +D; <= 200 mm +T +T - thickness; +A - area≥110≥270≥12
Extruded bars/rods +F, > 25 <= 250 mm +D; > 200 <= 250 mm +T +D - diametar; +T - thickness≥100≥260≥12
Extruded tubes, Annealed +O, all sizes≥125≥270≥12
Extruded tubes, Strain-hardened only +H111, all sizes≥110≥270≥12
Extruded tubes +H112, all sizes≥125≥270≥12
Extruded tubes +F, all sizes≥110≥270≥12
extruded sections +H112, all sizes≥125≥270≥12
extruded profiles +F, all sizes≥110≥270≥12

Physical properties

-50.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
22.30

Typical physical values

DensityElastic modulusPoisson's ratioRemarks
2.60–2.9069.00–79.000.33Typical property values for aluminum alloys. These values are not taken from a published standard; they are indicative only and must not be used for design.

Similar grades

GradeRegionSystem
EN AW-AlMg45Mn07
EN AW-5083ItalyUNI
EN AW-AlMg45Mn07
EN AW-5083SpainUNE
EN AW-AlMg45Mn07
EN AW-5083SwitzerlandSNV
EN AW-AlMg45Mn07
EN AW-5083FinlandSFS
EN AW-AlMg45Mn07
EN AW-5083PolandPN
EN AW-AlMg45Mn07
EN AW-5083AustriaONORM
EN AW-AlMg45Mn07
EN AW-5083NorwayNS
EN AW-AlMg45Mn07
EN AW-5083BelgiumNBN
EN AW-AlMg45Mn07
EN AW-5083HungaryMSZ
EN AW-AlMg45Mn07
EN AW-5083GermanyDIN
EN AW-AlMg45Mn07
EN AW-5083Czech RepublicCSN
EN AW-AlMg45Mn07
EN AW-5083United KingdomB.S.
EN AW-AlMg45Mn07
EN AW-5083BulgariaBDS
EN AW-AlMg45Mn07
EN AW-5083RomaniaASRO
EN AW-AlMg45Mn07
EN AW-5083FranceAFNOR NF
SB-209 5083United StatesASME
EN AW-AlMg45Mn07
EN AW-5083European UnionEN