Germany · DIN

Ms63

DIN 17682:1966 — Round Spring Wires Made of Wrought Copper Alloys; Strength Properties; Technical Conditions of Delivery

Chemical composition

wt% · log scale
0.0010.010.1110100Al0.02Cu63.5 – 65Fe0.05Mn0.05Ni0.2Pb0.05Sb0.01Sn0.05Total Ni0.3Total oth.0.05
  • min – max range
  • typical value

Mechanical properties

value range by condition
Tensile strength Rm680.00Rounds, spring wires, Strain-hardened, 0.5 < t <= 2.0 mmTensile strength Rm637.00Rounds, spring wires, Strain-hardened, 2.0 < t <= 5.0 mmTensile strength Rm735.00Rounds, spring wires, Strain-hardened, t <= 0.5 mm

Chemical composition

ElementminmaxSimilarRemarks
Al0.02
Cu63.565
Fe0.05
Mn0.05
Ni0.2
Pb0.05
Sb0.01
Sn0.05
Total Ni0.3
Total oth.0.05
Zn​​Bal​​​​Bal​​

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Rounds, spring wires, Strain-hardened, 0.5 < t <= 2.0 mm680.00
Rounds, spring wires, Strain-hardened, 2.0 < t <= 5.0 mm637.00
Rounds, spring wires, Strain-hardened, t <= 0.5 mm735.00

Physical properties

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
8.40

Similar grades

GradeRegionSystem
CW508LGermanyDIN
CW507LGermanyDIN
C 2700 BEJapanJIS
C 2680 PJapanJIS
2.0321GermanyDIN
2.0335GermanyDIN