High-Temperature Shape Memory Nitinol Ribbon
-- — -
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.05 | |||
| Fe | 0.05 | |||
| H | 0.005 | |||
| Ni | 55 | 56 | ||
| O | 0.05 | |||
| Other | 0.01 | |||
| Ti | Bal | Bal |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| cold drawn tempered | ≥1210 UTS | ≥5 |
Physical properties
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 6.50 |
Similar grades
| Grade | Region | System |
|---|---|---|
| High-Temperature Shape Memory Nitinol | Global | Enterprise standard |