United States · ASME
SB-367 Grade TiPd-7B
ASME SB-367
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.1 | |||
| Fe | 0.2 | |||
| H | 0.015 | |||
| N | 0.05 | |||
| O | 0.4 | |||
| Others each | 0.1 | |||
| Pd | 0.12 | 0.25 | ||
| Ti | Bal | |||
| Total Others | 0.4 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| castings, As cast | ≥275 | ≥345 | ≥15 Lo=25.4mm | HR ≤96 Hardened 1038℃;HB ≤210 Hardened 1038℃ |