South Korea · KS
NCuC
KS D 6023:2012 — KS D 6023
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.35 | |||
| Cu | 26 | 33 | ||
| Fe | 3.5 | |||
| Mn | 1.5 | |||
| Ni | Bal | |||
| P | 0.03 | |||
| S | 0.03 | |||
| Si | 1.25 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| castings, As cast | ≥170 | ≥450 | ≥25 |