Spain · UNE

PSL2 Grade X60N

UNE EN ISO 3183

Chemical composition

ElementminmaxSimilarRemarks
C0.24
CE PcmProduct analysis C<=0.12%Product analysis C<=0.12%
CEVSeamless pipe with t>20.00mmSeamless pipe with t>20.00mm
Cr0.5
Cu0.5
Mn1.4For each reduction of 0.01% below the specified max.concentration for CFor each reduction of 0.01% below the specified max.concentration for C
Mo0.5
Nb0.05
Nb+Ti+V0.15
Ni0.5
P0.025
S0.015
Si0.45
Ti0.04
V0.1

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
seamless or welded steel tube d > 323.90mm, normalize-rolled, normalized , normalized or normalized or tempered415–565 Rp0.5520–760 Rp0.5/Rm ratio min.0.93