Chemical composition

ElementminmaxSimilarRemarks
Al0.0150.06Al totalAl total
C0.18For each reduction of 0.01% below the specified max.concentration for CFor each reduction of 0.01% below the specified max.concentration for C
CE Pcm0.25Product analysis C≤0.12%Product analysis C≤0.12%
CEV0.41Seamless pipe with t>20.00mmSeamless pipe with t>20.00mm
Cr0.3
Cu0.25
Mn1.4
Mo0.1
N0.012Al/N≥2:1Al/N≥2:1
Nb0.06
Ni0.3
P0.025
S0.015
Si0.45
Ti0.05
V0.06

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel tubes;25 < t ≤ 40 mm, thermomechanically rolled360–510 Rp0.5460–760 Rt0.5/Rm ratio max.0.85≥20 These values apply to trans.test pieces taken from the pipe body.when long.test pieces are tested