Germany · DIN
2.4886
DIN 1736-2
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.02 | |||
| Cr | 14.5 | 16.5 | ||
| Fe | 4 | 7 | ||
| Mn | 1 | |||
| Mo | 15 | 17 | ||
| Ni | 50 | Up to 1% of Ni may be present as Co | ||
| Other | 0.5 | |||
| S | 0.015 | |||
| Si | 0.08 | |||
| V | 0.4 | |||
| W | 3 | 4.5 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| steel bars, welding electrodes, wire, welded condition | 400 | 700 | 25 | 60 |
Physical properties
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 8.80 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 7.90–8.80 | 185.00–205.00 | 0.32–0.34 | Nickel alloy:incoalloy |
| 7.86 | 190.00–210.00 | 0.27–0.30 | Material properties for low-carbon, high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design. |