International standard · ISO

6262A

ISO 6362-2:2012 — ISO 6362-2

Chemical composition

wt% · log scale
0.010.1110Bi0.4 – 0.9Cr0.04 – 0.14Cu0.15 – 0.4Fe0.7Mg0.8 – 1.2Mn0.15Others Total0.15Others each0.05Si0.4 – 0.8Sn0.4 – 1Ti0.1Zn0.25
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≤240 MPaTensile strength Rm≤260 MPaElongation A≤10 %Extruded bars, rods, solution heat treated artificially aged, D <= 220 or S <= 155 mmYield strength Rp0.2≥240 MPaTensile strength Rm≥260 MPaElongation A≥10 %extruded profiles, solution heat treated artificially aged, t <= 25 mm

Chemical composition

ElementminmaxSimilarRemarks
Al​​Bal​​
Bi0.40.9
Cr0.040.14
Cu0.150.4
Fe0.7
Mg0.81.2
Mn0.15
Others Total0.15
Others each0.05
Si0.40.8
Sn0.41
Ti0.1
Zn0.25

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Extruded bars, rods, solution heat treated artificially aged, D <= 220 or S <= 155 mm≤240≤260≤10
extruded profiles, solution heat treated artificially aged, t <= 25 mm≥240≥260≥10 Lo = 5.65√So; A <= 8% in Lo = 50mm