International standard · ISO

20 Cr 4

ISO 683-17:1999 — ISO 683-17

Chemical composition

wt% · log scale
0.0010.010.1110Al0.05C0.17 – 0.23Cr0.9 – 1.2Cu0.3Mn0.6 – 0.9P0.025S0.015Si0.4
  • min – max range
  • typical value

Mechanical properties

value range by condition
HardnessHB+ACHardnessHBRod, coil, ring, tube isothermal treated ferrite - hardness range of the pearlitic structure (+ FP)HardnessSteel coilbars, steel bars +HR, HBHardnessSteel bar annealed (+A)bars, HB

Chemical composition

ElementminmaxSimilarRemarks
Al0.05
C0.170.23
Cr0.91.2
Cu0.3
Mn0.60.9
P0.025
S0.015Where machinability is of primary importance
Si0.4

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
+ACHB ≤170
Rod, coil, ring, tube isothermal treated ferrite - hardness range of the pearlitic structure (+ FP)HB 140–187
bars, steel bars +HR, HBSteel coil 156.00
bars, HBSteel bar annealed (+A) 207

Heat treatment

Type1
Heat-treatment curveHardenability