Russia · GOST
10H17N13M2T
GOST 5949:1975 — GOST 5949
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionPhysical properties
vs. temperatureChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.1 | |||
| Cr | 16 | 18 | ||
| Mn | 2 | |||
| Mo | 2 | 3 | ||
| Ni | 12 | 14 | ||
| P | 0.035 | |||
| S | 0.02 | |||
| Si | 0.8 | |||
| Ti | 0.7 | 5 x %C <= 0.7% |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| Condition not stated | ≥215 | ≥510 | ≥40 |
Physical properties
20.0
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 206.00 | 15.00 | 504.00 | 0.75 | 7.90 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 7.61–8.10 | 190.00–215.00 | 0.27–0.30 | Typical material properties for stainless steel. These values are not taken from the standard; they are indicative and must not be used for design. |
| 7.86 | 190.00–210.00 | 0.27–0.30 | Material properties for low-carbon, high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design. |
Similar grades
| Grade | Region | System |
|---|---|---|
| Remanit 4571 IM | Global | Enterprise standard |
| Remanit 4571 | Global | Enterprise standard |
| IMCO316T | Global | Enterprise standard |
| CLC 17-12-2Ti | Global | Enterprise standard |
| Type 316Ti | Global | Enterprise standard |
| BÖHLER A300 | Global | Enterprise standard |
| 1.4571 | EN | |
| X 6 CrNiMoTi 17 12 2 | EN | |
| X 6 CrNiMoTi 17 12 2 | DIN | |
| 1.4571 | DIN | |
| 1Cr18Ni12Mo3Ti | GB | |
| 1Cr18Ni12Mo2Ti | GB |