China · GB

50CrVA

GB/T 3077:1999 — Alloy structure steels

Chemical composition

ElementminmaxSimilarRemarks
C0.470.54
Cr0.81.1
Cu0.25
Mn0.50.8
Mo0.1
Ni0.3
P0.025
S0.025
Si0.170.37
V0.10.2

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
bars, quenched and tempered, d <=, 25 mm≥1130≥1280≥10≥40HB ≤255 HB100/3000

Heat treatment

Type34Remarks
Heat-treatment processTempered加热温度500℃,冷却剂水、油表中所列热处理温度允许调整范围:淬火±15℃,低温回火±20℃,高温回火±50℃。
Heat-treatment processQuenched第一次淬火860℃,冷却剂油表中所列热处理温度允许调整范围:淬火±15℃,低温回火±20℃,高温回火±50℃。