Germany · WL
1.6944
WL 1.6944-4:1984 — WL 1.6944-4
Chemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.35 | 0.4 | ||
| Cr | 0.65 | 0.9 | ||
| Mn | 0.5 | 0.8 | ||
| Mo | 0.3 | 0.4 | ||
| Ni | 1.65 | 2 | ||
| P | 0.01 | |||
| S | 0.01 | |||
| Si | 0.15 | 0.35 | ||
| V | 0.08 | 0.15 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| annealed | ≤880 |
Physical properties
20.0
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 203.00 | 38.00 | 460.00 | 0.32 | 7.85 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 7.85 | 200.00–207.00 | 0.27–0.30 | 低碳钢低合金钢的材料性能属性数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。 |