Germany · DIN

MK 101

DIN 17222:1979 — DIN 17222

Chemical composition

wt% · log scale
0.010.1110C0.98 – 1.05Mn0.35 – 0.45P0.035S0.035Si0.15 – 0.25
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥1700 MPaTensile strength Rm1800–2400 MPaElongation A≥5 %HardnessHR+H+AYield strength Rp0.2≥320 MPaTensile strength Rm≥700 MPaElongation A≥25 %HardnessHB+G

Chemical composition

ElementminmaxSimilarRemarks
C0.981.05
Mn0.350.45
P0.035
S0.035
Si0.150.25

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
+H+A≥17001800–2400≥5 Lo = 5 x dHR 51–58 HRC
+G≥320≥700≥25 Lo = 5xDHB ≤220 HB30