Germany · DIN

12 Ni 19

DIN 17280:1987 — Steels with low temperature toughness; technical delivery conditions for plate, sheet, strip, wide flats, sections, bars and forgings

Chemical composition

ElementminmaxSimilarRemarks
C0.15
Mn0.30.8
Ni4.55.3
P0.025
S0.02
Si0.35
V0.05

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
+N, 30 < s <= 50 mm, 45 < d <= 75 mm≤380≤510≤19≤50;≤70
+N, s <= 30 mm, d <= 45 mm≤390≤510≤19≤50;≤70
+N or +A, 30 < s <= 50 mm, 45 < d <= 75 mm≤380≤510≤19≤50;≤70
+N or +A, s <= 30 mm, d <= 45 mm≤390≤510≤19≤50;≤70
+H+A, 30 < s <= 50 mm, 45 < d <= 75 mm≤380≤510≤19≤50;≤70
+H+A, s <= 30 mm, d <= 45 mm≤390≤510≤19≤50;≤70