European Union · EU

FeE 690 V KW

EU 137

Chemical composition

wt% · log scale
0.0010.010.1110B0.005C0.2Cr2Cu1.5Mn2Mo1N0.02Nb0.1Ni2P0.025S0.025Si1Ti0.2V0.2Zr0.15
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≤690 MPaTensile strength Rm≤790 MPaImpact energy Kv/Ku≤40 JElongation A≤15 %

Chemical composition

ElementminmaxSimilarRemarks
B0.005
C0.2
Cr2
Cu1.5
Mn2
Mo1
N0.02
Nb0.1
Ni2
P0.025
S0.025
Si1
Ti0.2
V0.2
Zr0.15

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
flats, heavy plate, quenched and tempered or precipitation hardened, >= 3 <= 50 mm≤690≤790≤15≤40