European Union · EN

1.4542

EN 10088-4:2009 — EN 10088-4

Chemical composition

wt% · log scale
0.0010.010.1110100C0.07Cr15 – 17Cu3 – 5Mn1.5Mo0.6Nb0.45Ni3 – 5P0.04S0.015Si0.7
  • min – max range
  • typical value

Mechanical properties

value range by condition
Tensile strength Rm≤1275 MPaElongation A≥5 %cold-rolled strip +AT, t < 8mmYield strength Rp0.2≥1150 MPaTensile strength Rm≥1300 MPaElongation A≥3 %cold-rolled strip +P1300, t < 8mmYield strength Rp0.2≥700 MPaTensile strength Rm≥900 MPaElongation A≥6 %cold-rolled strip +P900, t < 8mmYield strength Rp0.2≥1000 MPaTensile strength Rm1070–1270 MPaElongation A≥8 %hot-rolled heavy plate +P1070, t < 50mm

Physical properties

vs. temperature
Elastic modulus GPa
170 – 200°C
Mean thermal expansion 10⁻⁶/K
10.9 – 11.1°C

Chemical composition

ElementminmaxSimilarRemarks
C0.07
Cr1517
Cu35
Mn1.5
Mo0.6
Nb0.45>= 5 x %C
Ni35
P0.04
S0.015For machinability %S=0
Si0.7

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
cold-rolled strip +AT, t < 8mm≤1275≥5 Elongation after fracture; for t < 3mm and Lo=80mm or for t >= 3mm and Lo=50mm;
cold-rolled strip +P1300, t < 8mm≥1150≥1300≥3 Elongation after fracture; for t < 3mm and Lo=80mm or for t >= 3mm and Lo=50mm;
cold-rolled strip +P900, t < 8mm≥700≥900≥6 Elongation after fracture; for t < 3mm and Lo=80mm or for t >= 3mm and Lo=50mm;
hot-rolled heavy plate +P1070, t < 50mm≥10001070–1270≥8 Elongation after fracture; for t < 3mm and Lo=80mm or for t >= 3mm and Lo=50mm; Long. + tr. direction.
hot-rolled heavy plate +P850, t < 50mm≥600850–1050≥12 Elongation after fracture; for t < 3mm and Lo=80mm; Amin.=12% for t >= 3mm and Lo=50mm; Long. + tr. direction.
hot-rolled heavy plate +P950, t < 50mm≥800950–1150≥10 Elongation after fracture; for t < 3mm and Lo=80mm; Amin.=10% for t >= 3mm and Lo=50mm; Long. + tr. direction.
hot-rolled heavy plate +SR630, t < 50mm≤1050

Physical properties

20.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
200.0016.00500.000.717.80

Typical physical values

DensityElastic modulusPoisson's ratioRemarks
7.61–8.10190.00–215.000.27–0.30Typical material properties for stainless steel. These values are not taken from the standard; they are indicative and must not be used for design.
7.86190.00–210.000.27–0.30Material properties for low-carbon, high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design.

Heat treatment

Type1
Heat-treatment curveCCT

Similar grades

GradeRegionSystem
4542-174-00-IInternational standardISO
S51740ChinaGB
05Cr17Ni4Cu4NbChinaGB
A564 S17400United StatesASTM
A693 S17400United StatesASTM
1.4542ItalyUNI
X 5 CrNiCuNb 16 4ItalyUNI
1.4542SpainUNE
X 5 CrNiCuNb 16 4SpainUNE
1.4542RomaniaSTAS
X 5 CrNiCuNb 16 4RomaniaSTAS
1.4542SwedenSS
X 5 CrNiCuNb 16 4SwedenSS
1.4542SwitzerlandSNV
X 5 CrNiCuNb 16 4SwitzerlandSNV
1.4542FinlandSFS
X 5 CrNiCuNb 16 4FinlandSFS
1.4542PolandPN
X 5 CrNiCuNb 16 4PolandPN
1.4542AustriaONORM
X 5 CrNiCuNb 16 4AustriaONORM
1.4542NorwayNS
X 5 CrNiCuNb 16 4NorwayNS
1.4542BelgiumNBN
X 5 CrNiCuNb 16 4BelgiumNBN
1.4542HungaryMSZ
X 5 CrNiCuNb 16 4HungaryMSZ
1.4542Czech RepublicCSN
X 5 CrNiCuNb 16 4Czech RepublicCSN
1.4542BulgariaBDS
X 5 CrNiCuNb 16 4BulgariaBDS
1.4542United KingdomB.S.
X 5 CrNiCuNb 16 4United KingdomB.S.
1.4542FranceAFNOR NF
PK346GlobalEnterprise standard
EskyLos 4542GlobalEnterprise standard
Remanit 4542GlobalEnterprise standard
IMCO630GlobalEnterprise standard
VIRGO 17.4 PHGlobalEnterprise standard
BÖHLER N700 ISOEXTRAGlobalEnterprise standard
Project 70+ Custom 630 StainlessGlobalEnterprise standard
Carpenter Stainless Custom 630GlobalEnterprise standard
Carpenter Stainless 17Cr-4NiGlobalEnterprise standard
X5CrNiCuNb16-4International standardISO
S17400United StatesUNS
17-4PHUnited StatesSAE
X 5 CrNiCuNb 16 4FranceAFNOR NF
X 5 CrNiCuNb 16 4GermanyDIN
1.4542GermanyDIN