European Union · EN

1.0225

EN 10296-1:2003 — EN 10296-1

Chemical composition

wt% · log scale
0.010.1110C0.21Mn1.4P0.045S0.045Si0.35
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥275 MPaTensile strength Rm≥410 MPaElongation A≥21 %steel tubes +N, t <=, 40 mmYield strength Rp0.2≥340 MPaTensile strength Rm≥440 MPaElongation A≥6 %steel tubes +U, t <=, 40 mmTensile strength Rm≥390 MPaElongation A≥21 %steel tubes +A, t <=, 40 mm

Chemical composition

ElementminmaxSimilarRemarks
C0.21
Mn1.4
P0.045
S0.045
Si0.35

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
steel tubes +N, t <=, 40 mm≥275 Proof stress is Upper yield stress≥410≥21
steel tubes +U, t <=, 40 mm≥340 Proof stress is Upper yield stress≥440≥6
steel tubes +A, t <=, 40 mm≥390≥21