France · AFNOR NF
38 MB 5
NF A37-504
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| B | 0.0008 | 0.005 | ||
| C | 0.35 | 0.4 | ||
| Fe | Bal | |||
| Mn | 1.1 | 1.4 | ||
| P | 0.035 | |||
| S | 0.025 | |||
| Si | 0.1 | 0.4 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| bars, coil, steel strip, quenched and tempered | 860.00 | |||||
| bars, steel strip, annealed, > 0.5 <= 3 mm, coil | 640.00 | 18 | ||||
| bars, steel strip, annealed, > 0.5 <= 3 mm, HR | Coil 92.00 |
Heat treatment
| Type | 1 |
|---|---|
| Heat-treatment curve | Hardness-Tempering |
| Heat-treatment curve | Hardenability |
| Heat-treatment curve | CCT |