France · AFNOR NF
XC 18
NF A37-503
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionPhysical properties
vs. temperatureChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.16 | 0.22 | ||
| Mn | 0.4 | 0.7 | ||
| P | 0.035 | |||
| S | 0.025 | |||
| Si | 0.15 | 0.35 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| bars, steel strip, annealed, > 0.5 <= 3 mm, coil | 430.00 | 27 | ||||
| bars, steel strip, annealed, > 0.5 <= 3 mm, HR | 卷板 76.00 |
Physical properties
20.0
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 210.00 | 58.00 | 460.00 | 0.11 | 7.85 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 7.86 | 203.00 | 0.27–0.30 | 低碳,低合金钢的典型性能数值。此值不来源于标准,它是指示性指标,不能被用于设计用途。 |
Heat treatment
| Type | 1 |
|---|---|
| Heat-treatment curve | TTT |