France · AFNOR NF

TU 10 CD 5-05

NF A49-215

Chemical composition

wt% · log scale
0.010.1110C0.17Cr0.9 – 1.6Cu0.25Mn0.2 – 0.7Mo0.41 – 0.69Ni0.3P0.035S0.035Si0.45 – 1.05Sn0.03
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≤225 MPaTensile strength Rm≤440 MPaElongation A≤22 %Yield strength Rp0.2≤325 MPaTensile strength Rm≤490 MPaElongation A≤20 %seamless steel tube, steel tubes, heat treatedHardness钢管  热处理 (HT2)Hardness钢管  热处理 (HT1)seamless steel tube, HR

Chemical composition

ElementminmaxSimilarRemarks
C0.17
Cr0.91.6
Cu0.25
Mn0.20.7
Mo0.410.69
Ni0.3
P0.035
S0.035
Si0.451.05
Sn0.03

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
seamless steel tube, steel tubes, heat treated≤225;≤325≤440;≤490≤22;≤20
seamless steel tube, HR钢管  热处理 (HT2) ≤93;钢管  热处理 (HT1) ≤90