Italy · UNI
C 40
UNI 7065:1972 — UNI 7065
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.38 | 0.43 | ||
| Mn | 0.4 | 0.65 | ||
| P | 0.02 | |||
| S | 0.02 | |||
| Si | 0.35 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| steel strip, annealed | ≤510 | ≥21 L0=80 mm | HR ≤76 HRB;HB ≤135 HRB |
Heat treatment
| Type | 1 |
|---|---|
| Heat-treatment curve | Hardness-Tempering |