Japan · JIS
FCA-NiCr 20 2
JIS G5510:2012 — Austenitic iron castings
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 3 | |||
| Cr | 1 | 2.5 | ||
| Cu | 0.5 | |||
| Mn | 0.5 | 1.5 | ||
| Ni | 18 | 22 | ||
| P | 0.25 | |||
| Si | 1 | 2.8 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| castings | 170–210 | 2–3 | HB 120–215 HBW |
Physical properties
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 18.70 | 1.40 | 7.30 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 6.80–7.90 | 100.00–190.00 | 0.26–0.30 | Material properties for cast iron. These values are not taken from the standard; they are indicative and must not be used for design. |
Similar grades
| Grade | Region | System |
|---|---|---|
| AFG Ni13Mn7 | IS | |
| FCA-NiCuCr 15 6 3 | JIS | |
| GGL-NiCr 20 2 | DIN | |
| 0.6660 | DIN | |
| F2 | B.S. |