Russia · GOST

35

GOST 8479:1970 — GOST 8479

Chemical composition

ElementminmaxSimilarRemarks
C0.320.4
Cr0.25
Mn0.50.8
P0.035
S0.04
Si0.170.37

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
forgings, Heat treated , > 500 <= 800 mm≥20≥49 KCUHB 101–143

Physical properties

20.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
206.007.83

Typical physical values

DensityElastic modulusPoisson's ratioRemarks
7.80202.000.27–0.30低碳无合金钢的材料性能属性数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。

Heat treatment

Type1
Heat-treatment curve淬透性
Heat-treatment curveTempered

Similar grades

GradeRegionSystem
S 35 CJapanJIS
Ck 35GermanySEW
C 35 EGermanyDIN
Ck 35GermanyDIN
Cq 35GermanyDIN
1.1181GermanyDIN