United States · SAE
301
SAE J 405:1998 — SAE J 405
Chemical composition
wt% · log scale- min – max range
- typical value
Physical properties
vs. temperatureChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.15 | |||
| Cr | 16 | 18 | ||
| Mn | 2 | |||
| N | 0.1 | |||
| Ni | 6 | 8 | ||
| P | 0.045 | |||
| S | 0.03 | |||
| Si | 1 |
Physical properties
20.0
| Elastic modulus | Mean thermal expansion | Thermal conductivity | Specific heat | Resistivity | Density | Poisson's ratio |
|---|---|---|---|---|---|---|
| 186.00;179.00;200.00 | 7.92 | 0.27 |
Typical physical values
| Density | Elastic modulus | Poisson's ratio | Remarks |
|---|---|---|---|
| 7.61–8.10 | 190.00–215.00 | 0.27–0.30 | 不锈钢的典型材料性能数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。 |
| 7.86 | 190.00–210.00 | 0.27–0.30 | 低碳,高合金钢材料性能属性数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。 |
Fatigue
1.薄板; 退火; Bending; T: 20°C; Rotating beam; 方向: L
| Item | Detail |
|---|---|
| Product | sheet; annealed |
| Experiment | Bending; T: 20°C |
| Specimen | Rotating beam; Direction: L |
| Property | Value |
|---|---|
| Elastic modulus (GPa) | 200.0 |
| Yield strength (MPa) | 276.0 |
| Tensile strength (MPa) | 827.0 |
| Elongation (%) | 75.0 |
| Hardness (HRB) | 80.0 |
| No. | Specimen | Cycles |
|---|---|---|
| 1 | Rotating beam; Direction: L | E6 |
Similar grades
| Grade | Region | System |
|---|---|---|
| 4310-301-00-I | International standard | ISO |
| 4319-301-00-I | International standard | ISO |
| X5CrNi17-7 | International standard | ISO |
| SA-240 S30100 | ASME | |
| SA-240 Type 301 | ASME | |
| S30110 | GB | |
| 12Cr17Ni7 | GB | |
| 30301 | AMS | |
| X10CrNi18-8 | International standard | ISO |
| S30100 | UNS | |
| 30301 | SAE | |
| 1H18N9 | PN | |
| SUS 301L | JIS | |
| SUS 301 | JIS | |
| X 12 CrNi 17 07 | UNI | |
| 1.4319 | EN | |
| 1.4310 | EN | |
| 1.4318 | EN | |
| X5CrNi17-7 | EN | |
| X 2 CrNiN 18 7 | EN | |
| X 10 CrNi 18 8 | EN |