Romania · STAS
K55
SR EN ISO 11960
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| P | 0.03 | |||
| S | 0.03 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| Casing and tubing, Heat treated | 379–552 | ≥655 Total elongation under load:0.5% | 12–20 Lo=50.80mm |