United States · ASTM
A304 8625 H
ASTM A304:1996 — Standard Specification for Steel Bars Subject to End-Quench Hardenability Requirements
Chemical composition
wt% · log scale- min – max range
- typical value
Chemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| C | 0.22 | 0.28 | ||
| Cr | 0.35 | 0.65 | ||
| Mn | 0.6 | 0.95 | ||
| Mo | 0.15 | 0.25 | ||
| Ni | 0.35 | 0.75 | ||
| P | 0.035 | |||
| S | 0.04 | |||
| Si | 0.15 | 0.35 |
Heat treatment
| Type | 1 |
|---|---|
| Heat-treatment curve | Hardenability |