Global · Enterprise standard
E36
-- — -
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionChemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| Al | 0.02 | |||
| C | 0.18 | |||
| Cr | 0.2 | |||
| Cu | 0.35 | |||
| Mn | 0.9 | 1.6 | ||
| Mo | 0.08 | |||
| Nb | 0.02 | 0.05 | ||
| Ni | 0.4 | |||
| P | 0.35 | |||
| S | 0.35 | |||
| Si | 0.5 | |||
| Ti | 0.02 | |||
| V | 0.05 | 0.1 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| hot rolled | ≥355 | 490–620 | ≥21 Lo = 5 mm. | ≥34 KvL; KvT = 24 J for t <= 50 mm; KvL = 41J and KvT =27J for 50 < t <=70 mm; KvL = 50J and KvT =34J for 70 < t <= 100mm; Testing temperature T = -40°C; |
High/low temperature
| Condition | Temperature ℃ | min | Remarks |
|---|---|---|---|
| hot rolled | -40 | 34 | KvL; KvT = 24 J for t <= 50 mm; KvL = 41J and KvT =27J for 50 < t <=70 mm; KvL = 50J and KvT =34J for 70 < t <= 100mm |