Global · Enterprise standard

IMCO321

-- — -

Chemical composition

wt% · log scale
0.010.1110100C0.02Cr17.2Mn1.5Mo0.3Ni9.1P0.03S0.025Si0.5
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥190 MPaTensile strength Rm500–700 MPaElongation A≥40 %Reduction of area Z≥50 %HardnessHB

Physical properties

vs. temperature
Mean thermal expansion 10⁻⁶/K
16.5 – 18.5°C

Chemical composition

ElementminmaxSimilarRemarks
C0.02
Cr17.2
Mn1.5
Mo0.3
Ni9.1
P0.03
S0.025
Si0.5
Ti5XC

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Solution treated≥190500–700≥40 for A5; max 13 % for A10≥50HB ≤215 HRB

Physical properties

20.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
200.0014.60500.000.737.90

Typical physical values

DensityElastic modulusPoisson's ratioRemarks
7.61–8.10190.00–215.000.27–0.30不锈钢的典型材料性能数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。
7.86190.00–210.000.27–0.30低碳,高合金钢材料性能属性数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。

Similar grades

GradeRegionSystem
PK11SPGlobalEnterprise standard
Remanit 4541 IMGlobalEnterprise standard
Remanit 4541GlobalEnterprise standard
Remanit 4462GlobalEnterprise standard
NIROSTA 4462GlobalEnterprise standard
URANUS 45NGlobalEnterprise standard
CLC 18-10TiGlobalEnterprise standard
Type 321GlobalEnterprise standard
SANMAC SAF 2205GlobalEnterprise standard
Sandvik 321GlobalEnterprise standard
BÖHLER A903 EXTRAGlobalEnterprise standard
BÖHLER A700GlobalEnterprise standard
Carpenter Stainless Type 321GlobalEnterprise standard
Carpenter 2205 StainlessGlobalEnterprise standard
SUS 321JapanJIS
X 6 CrNiTi 18 11ItalyUNI
1.4878European UnionEN
1.4541European UnionEN
1.4462European UnionEN
X 6 CrNiTi 18 10European UnionEN
X 8 CrNiTi 18 10GermanyDIN
X 6 CrNiTi 18 10GermanyDIN
X 2 CrNiMoN 22 5 3GermanyDIN
1.4544GermanyWL
1.4541GermanyDIN
1.4462GermanyDIN