Global · Enterprise standard

HU

-- — -

Mechanical properties

value range by condition
Tensile strength Rm≥448 MPaElongation A≥4 %

Physical properties

vs. temperature
Mean thermal expansion 10⁻⁶/K
15.8 – 19.1°C
Thermal conductivity W/(m·K)
12.1 – 26.5°C

Chemical composition

ElementminmaxSimilarRemarks
C0.4
Cr19
Mn0.3
Ni39
Si1

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
castings, As cast≥448≥4 Lo = 30 mm

Physical properties

20.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
8.03

Typical physical values

DensityElastic modulusPoisson's ratioRemarks
7.85200.00–207.000.27–0.30低碳钢低合金钢的材料性能属性数值,此值不来源于标准,它是指示性指标,不能被用于设计用途。