United States · ABS

AB/2

-- — -

Chemical composition

wt% · log scale
0.010.11C0.35Mn0.035P0.035
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥205 MPaTensile strength Rm≥415 MPaElongation A≥24 %forgings, > 305 mm, Heat treatedYield strength Rp0.2≥205 MPaTensile strength Rm≥415 MPaElongation A≥25 %forgings, <= 305 mm, Heat treated

Chemical composition

ElementminmaxSimilarRemarks
C0.35
Mn0.035
P0.035

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
forgings, > 305 mm, Heat treated≥205≥415≥24
forgings, <= 305 mm, Heat treated≥205≥415≥25