Switzerland · SNV

1.7033

SN EN 10250-3

Chemical composition

wt% · log scale
0.010.1110C0.3 – 0.37Cr0.9 – 1.2Mn0.6 – 0.9P0.035S0.035Si0.4
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2460 MPaTensile strength Rm700 MPaImpact energy Kv/Ku40 JElongation A15 %

Chemical composition

ElementminmaxSimilarRemarks
C0.30.37
Cr0.91.2
Mn0.60.9
P0.035
S0.035
Si0.4

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
die forgings, forgings, quenched and tempered, <= 70 mm, forged bars4607001540

Heat treatment

Type1
Heat-treatment curveHardness-Tempering
Heat-treatment curveCCT
Heat-treatment curveTTT
Heat-treatment curveHardenability