Romania · STAS

1.4016

SR EN 10088-2

Chemical composition

wt% · log scale
0.0010.010.1110100C0.08Cr16 – 18Mn1P0.04S0.015Si1
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥280 MPaTensile strength Rm450–600 MPaElongation A≥20 %Yield strength Rp0.2≥260 MPaTensile strength Rm450–600 MPaElongation A≥20 %cold-rolled strip, annealed, <= 6 mmYield strength Rp0.2≥260 MPaTensile strength Rm430–630 MPaElongation A≥20 %Yield strength Rp0.2≥240 MPaTensile strength Rm430–630 MPaElongation A≥20 %hot-rolled heavy plate, annealed, <= 25 mmYield strength Rp0.2≥260 MPaTensile strength Rm450–600 MPaElongation A≥18 %Yield strength Rp0.2≥240 MPaTensile strength Rm450–600 MPaElongation A≥18 %hot-rolled strip, annealed, <= 12 mm

High / low temperature

value vs. temperature
186196205214224100150200250300350400°C
  • Condition not stated · Yield strength Rp0.2

Physical properties

vs. temperature
Elastic modulus GPa
195 – 220°C
Mean thermal expansion 10⁻⁶/K
10.0 – 11.0°C
Thermal conductivity W/(m·K)
23.4 – 26.9°C
Specific heat J/(kg·K)
460 – 760°C
Resistivity Ω·mm²/m
0.600 – 1.25°C
Density kg/dm³
7.70 – 7.75°C

Chemical composition

ElementminmaxSimilarRemarks
C0.08
Cr1618
Mn1
P0.04
S0.015For bars
Si1

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
cold-rolled strip, annealed, <= 6 mm≥280;≥260450–600≥20 For t < 3 mm
hot-rolled heavy plate, annealed, <= 25 mm≥260;≥240430–630≥20 For t < 3 mm
hot-rolled strip, annealed, <= 12 mm≥260;≥240450–600≥18 For t < 3 mm

Physical properties

20.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
220.00;210.0025.00460.000.607.70;7.75

Typical physical values

DensityElastic modulusPoisson's ratioRemarks
7.61–8.10190.00–215.000.27–0.30Typical material properties for stainless steel. These values are not taken from the standard; they are indicative and must not be used for design.
7.86190.00–210.000.27–0.30Material properties for low-carbon, high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design.

High/low temperature

Yield strength Rp0.2 (MPa)
Temperature ℃Approx.
400190
350195
300200
250205
200210
150215
100220

Heat treatment

Type1
Heat-treatment curveTTT

Similar grades

GradeRegionSystem
1.4016ItalyUNI
X 6 Cr 17ItalyUNI
1.4016SpainUNE
X 6 Cr 17SpainUNE
X 6 Cr 17RomaniaSTAS
1.4016SwedenSS
X 6 Cr 17SwedenSS
1.4016SwitzerlandSNV
X 6 Cr 17SwitzerlandSNV
1.4016FinlandSFS
X 6 Cr 17FinlandSFS
1.4016PolandPN
X 6 Cr 17PolandPN
1.4016AustriaONORM
X 6 Cr 17AustriaONORM
1.4016NorwayNS
X 6 Cr 17NorwayNS
1.4016BelgiumNBN
X 6 Cr 17BelgiumNBN
1.4016HungaryMSZ
X 6 Cr 17HungaryMSZ
1.4016Czech RepublicCSN
X 6 Cr 17Czech RepublicCSN
1.4016BulgariaBDS
X 6 Cr 17BulgariaBDS
1.4016United KingdomB.S.
X 6 Cr 17United KingdomB.S.
1.4016FranceAFNOR NF
X 6 Cr 17FranceAFNOR NF
X 6 Cr 17GermanyDIN
1.4016GermanyDIN