Spain · UNE
1.0452
UNE EN 10216-4
Chemical composition
wt% · log scale- min – max range
- typical value
Mechanical properties
value range by conditionHigh / low temperature
value vs. temperature- Seamless tubes quenched and tempered +QT 25 < T <= 40 mm +T · Impact energy Kv/Ku
- Seamless tubes quenched and tempered +QT T <= 25 mm +T · Impact energy Kv/Ku
Chemical composition
| Element | min | max | Similar | Remarks |
|---|---|---|---|---|
| Al | 0.02 | By agreement between purchaser and manufacturer | ||
| C | 0.17 | |||
| Cr | 0.3 | |||
| Cu | 0.3 | In order to facilitate subsequent forming operation | ||
| Mn | 0.4 | 1.2 | ||
| Mo | 0.08 | |||
| Nb | 0.01 | |||
| Ni | 0.3 | |||
| P | 0.025 | |||
| S | 0.02 | |||
| Si | 0.35 | |||
| Ti | 0.04 | |||
| V | 0.02 |
Mechanical properties
| Heat treatment / condition | Yield strength | Tensile strength | Elongation | Reduction of area | Impact energy | Hardness |
|---|---|---|---|---|---|---|
| Seamless tubes +QT, 25 < T <= 40 mm | ≥55 KV (20°C);≥45 KV (-20°C);≥40 KV (-40°C) | |||||
| Seamless tubes +QT, T <= 25 mm | ≥255 Upper yield stress is proof stress | 360–490 | ≥23 Long. direction | ≥60 KV (20°C);≥50 KV (-20°C);≥45 KV (-40°C);≥40 KV (-50°C) |
High/low temperature
| Condition | Temperature ℃ | min | Remarks |
|---|---|---|---|
| Seamless tubes quenched and tempered +QT 25 < T <= 40 mm +T | -20 | 45 | KV |
| Seamless tubes quenched and tempered +QT 25 < T <= 40 mm +T | -40 | 40 | KV |
| Seamless tubes quenched and tempered +QT T <= 25 mm +T | -20 | 50 | KV |
| Seamless tubes quenched and tempered +QT T <= 25 mm +T | -40 | 45 | KV |
| Seamless tubes quenched and tempered +QT T <= 25 mm +T | -50 | 40 | KV |