Finland · SFS

GS200

SFS EN 10340

Chemical composition

wt% · log scale
0.010.1110C0.18Cr0.3Cr+Mo+Ni+V+Cu1Cu0.3Mn1.2Mo0.12Ni0.4P0.03S0.025Si0.6V0.03
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥200 MPaTensile strength Rm380–530 MPaImpact energy Kv/Ku≥35 JElongation A≥25 %

Chemical composition

ElementminmaxSimilarRemarks
C0.18
Cr0.3
Cr+Mo+Ni+V+Cu1
Cu0.3
Mn1.2
Mo0.12
Ni0.4
P0.03
S0.025
Si0.6
V0.03

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
castings +N, <= 100 mm≥200380–530≥25≥35 KV ( room temperature)