France · AFNOR NF

EN-JM1030

NF EN 1562

Chemical composition

wt% · log scale
0.010.11P0.1
  • min – max range
  • typical value

Mechanical properties

value range by condition
Yield strength Rp0.2≥220 MPaTensile strength Rm≥400 MPaElongation A≥5 %HardnessHBHeat treated, 12 mmYield strength Rp0.2≥230 MPaTensile strength Rm≥420 MPaElongation A≥4 %Heat treated, 15 mmTensile strength Rm≥300 MPaElongation A≥12 %Heat treated, 6 mmYield strength Rp0.2≥200 MPaTensile strength Rm≥360 MPaElongation A≥8 %Heat treated, 9 mm

Chemical composition

ElementminmaxSimilarRemarks
Fe​​Bal​​
P0.1

Mechanical properties

Heat treatment / conditionYield strengthTensile strengthElongationReduction of areaImpact energyHardness
Heat treated, 12 mm≥220≥400≥5 Lo = 3.4 Sqrt (Cross Sectional Area)HB ≤220
Heat treated, 15 mm≥230≥420≥4 Lo = 3.4 Sqrt (Cross Sectional Area)
Heat treated, 6 mm≥300≥12 Lo = 3.4 Sqrt (Cross Sectional Area)
Heat treated, 9 mm≥200≥360≥8 Lo = 3.4 Sqrt (Cross Sectional Area)