China · GB

06Cr19Ni13Mo3

GB/T 20878:2007 — Stainless and heat resisting steels-- Designation and chemical composition

Chemical composition

wt% · log scale
0.010.1110100C0.08Cr18 – 20Mn2Mo3 – 4Ni11 – 15P0.045S0.03Si1
  • min – max range
  • typical value

Physical properties

vs. temperature
Mean thermal expansion 10⁻⁶/K
16.0 – 18.5°C
Thermal conductivity W/(m·K)
16.3 – 21.5°C

Chemical composition

ElementminmaxSimilarRemarks
C0.08
Cr1820
Mn2
Mo34
Ni1115
P0.045
S0.03
Si1

Physical properties

20.0

Elastic modulusMean thermal expansionThermal conductivitySpecific heatResistivityDensityPoisson's ratio
193.00500.000.748.00

Typical physical values

DensityElastic modulusPoisson's ratioRemarks
7.61–8.10190.00–215.000.27–0.30Typical material properties for stainless steel. These values are not taken from the standard; they are indicative and must not be used for design.
7.86190.00–210.000.27–0.30Material properties for low-carbon, high-alloy steel. These values are not taken from the standard; they are indicative and must not be used for design.

Similar grades

GradeRegionSystem
4401-316-00-IInternational standardISO
NTK 317GlobalEnterprise standard
SA-813 S31700United StatesASME
SA-403 CR317United StatesASME
SA-403 S31700United StatesASME
SA-403 WP 317United StatesASME
S31668ChinaGB
022Cr19Ni13Mo3ChinaGB
S31703ChinaGB
S31708ChinaGB
X 3 CrNiMo 18-12-3GermanyDIN
X5CrNiMo17-12-2International standardISO
SA-813 TP317United StatesASME
SA-409 TP317United StatesASME
SA-182 F 317United StatesASME
SA-249 TP 317United StatesASME
SA-240 S31700United StatesASME
SA-312 Grade TP 317United StatesASME
1.4449European UnionEN
1.4401European UnionEN
X 3 CrNiMo 18-12-3European UnionEN
X 5 CrNiMo 17 12 2European UnionEN
1.4449GermanyDIN
0Cr19Ni13Mo3ChinaGB
0Cr18Ni12Mo3TiChinaGB
00Cr19Ni13Mo3ChinaGB